Abstract
This paper presents the initial results of research on possibilities for utilization of copper smelting slag from Eti Bakir Kastamonu Küre Plant, Turkey for producing colourful crystal ceramic glazes. The compositions were formulated using the Seger method and applied in the commercial porcelain bodies which were fired at 1200 °C. Different amounts of wastes were added into the glaze compositions and applied in dry form to porcelain body. Suitable firing temperature was 1200 °C for 3 h. Copper smelting slag was characterized by XRD and DTA-TG. Glazes were characterized by SEM-EDX. The initial study has shown that copper smelting slag is suitable for obtaining artistic glazes based on Li2O-ZnO system and bringing the attractive colours to the ceramic glazes.
Keywords
Download Citation
Endnote/Zotero/Mendeley (RIS)BibTeX
- B. Gorai, R.K. Jana and Premchand, Resour. Conserv. Recycling, 39, 299 (2003); doi:10.1016/S0921-3449(02)00171-4.
- K.S. Al-Jabri, A.H. Al-Saidy and R. Taha, Constr. Build. Mater., 25, 933 (2011); doi:10.1016/j.conbuildmat.2010.06.090.
- I. Alp, H. Deveci and H. Süngün, J. Hazard. Mater., 159, 390 (2008); doi:10.1016/j.jhazmat.2008.02.056.
- D. Eliche-Quesada, F.A. Corpas-Iglesias, L. Pérez-Villarejo and F.J. Iglesias-Godino, Constr. Build. Mater., 34, 275 (2012); doi:10.1016/j.conbuildmat.2012.02.079.
- S.R. Prim, M.V. Folgueras, M.A. de Lima and D. Hotza, J. Hazard. Mater., 192, 1307 (2011); doi:10.1016/j.jhazmat.2011.06.034.
- W. Hajjaji, G. Costa, C. Zanelli, M.J. Ribeiro, M.P. Seabra, M. Dondi and J.A. Labrincha, J. Eur. Ceram. Soc., 32, 753 (2012); doi:10.1016/j.jeurceramsoc.2011.10.018.
- R.C. da Silva, S.A. Pianaro and S.M. Tebcherani, Ceram. Int., 38, 2725 (2012); doi:10.1016/j.ceramint.2011.11.041.
- M. Erol, A. Genç, M.L. Öveçoglu, E. Yücelen, S. Küçükbayrak and Y. Taptik, J. Eur. Ceram. Soc., 20, 2209 (2000); doi:10.1016/S0955-2219(00)00099-6.
- P. Appendino, M. Ferraris, I. Matekovits and M. Salvo, J. Eur. Ceram. Soc., 24, 803 (2004); doi:10.1016/S0955-2219(03)00264-4.
- A.R. Boccaccini, M. Bucker and J. Bossert, Tile & Brick Int., 12, 515 (1996).
- S.P. Raut, R.V. Ralegaonkar and S.A. Mandavgane, Constr. Build. Mater., 25, 4037 (2011); doi:10.1016/j.conbuildmat.2011.04.038.
- O.C. Pereira and A.M. Bernardin, J. Hazard. Mater., 233-234, 103 (2012); doi:10.1016/j.jhazmat.2012.06.057.
- S. Dakhai, L.A. Orlova and N.Y. Mikhailenko, Glass Ceram., 56, 177 (1999); doi:10.1007/BF02681330.
- A. Wannagon, S. Prasanphan and S. Sanguanpak, J. Eur. Ceram. Soc., 33, 653 (2013); doi:10.1016/j.jeurceramsoc.2012.10.027.
References
B. Gorai, R.K. Jana and Premchand, Resour. Conserv. Recycling, 39, 299 (2003); doi:10.1016/S0921-3449(02)00171-4.
K.S. Al-Jabri, A.H. Al-Saidy and R. Taha, Constr. Build. Mater., 25, 933 (2011); doi:10.1016/j.conbuildmat.2010.06.090.
I. Alp, H. Deveci and H. Süngün, J. Hazard. Mater., 159, 390 (2008); doi:10.1016/j.jhazmat.2008.02.056.
D. Eliche-Quesada, F.A. Corpas-Iglesias, L. Pérez-Villarejo and F.J. Iglesias-Godino, Constr. Build. Mater., 34, 275 (2012); doi:10.1016/j.conbuildmat.2012.02.079.
S.R. Prim, M.V. Folgueras, M.A. de Lima and D. Hotza, J. Hazard. Mater., 192, 1307 (2011); doi:10.1016/j.jhazmat.2011.06.034.
W. Hajjaji, G. Costa, C. Zanelli, M.J. Ribeiro, M.P. Seabra, M. Dondi and J.A. Labrincha, J. Eur. Ceram. Soc., 32, 753 (2012); doi:10.1016/j.jeurceramsoc.2011.10.018.
R.C. da Silva, S.A. Pianaro and S.M. Tebcherani, Ceram. Int., 38, 2725 (2012); doi:10.1016/j.ceramint.2011.11.041.
M. Erol, A. Genç, M.L. Öveçoglu, E. Yücelen, S. Küçükbayrak and Y. Taptik, J. Eur. Ceram. Soc., 20, 2209 (2000); doi:10.1016/S0955-2219(00)00099-6.
P. Appendino, M. Ferraris, I. Matekovits and M. Salvo, J. Eur. Ceram. Soc., 24, 803 (2004); doi:10.1016/S0955-2219(03)00264-4.
A.R. Boccaccini, M. Bucker and J. Bossert, Tile & Brick Int., 12, 515 (1996).
S.P. Raut, R.V. Ralegaonkar and S.A. Mandavgane, Constr. Build. Mater., 25, 4037 (2011); doi:10.1016/j.conbuildmat.2011.04.038.
O.C. Pereira and A.M. Bernardin, J. Hazard. Mater., 233-234, 103 (2012); doi:10.1016/j.jhazmat.2012.06.057.
S. Dakhai, L.A. Orlova and N.Y. Mikhailenko, Glass Ceram., 56, 177 (1999); doi:10.1007/BF02681330.
A. Wannagon, S. Prasanphan and S. Sanguanpak, J. Eur. Ceram. Soc., 33, 653 (2013); doi:10.1016/j.jeurceramsoc.2012.10.027.